23.01.2025

Milky film after laminating: will a second pass help?

Milky film after laminating: will a second pass help?

If glossy thermal laminating film comes out milky, compare the pouch thickness with the range of your pouch laminator, check the setting and wait until it is ready. If the pouch is flat and the print can take heat, run it through again: most often the adhesive simply did not get enough heat. If the film develops waves or the print changes colour, stop heating it.

Why a white haze remains over the print

There is a heat-activated adhesive between the clear film and the paper. Before heating it is always slightly cloudy; that is normal. In the laminator, the adhesive heats up and bonds the film to the print. With too little heat, a milky haze or patches remain over the image. Judge the item once it has cooled: hold it so that glare does not get in the way and look at the dark areas, where haze shows. Tiny bubbles or silvery specks on dark areas together with haze are the same under-heating; the same second pass removes them.

The adhesive between film and print changes

Not enough heat

Clear film
Adhesive remains cloudy
Print
Paper

Adhesive heated sufficiently

Clear film
Adhesive is clear; the bond has formed
Print
Paper

Cross-section of the upper half of a pouch: only the adhesive changes.

Check first: gloss or matte

A matte pouch diffuses reflections even when laminated correctly, and heat will not make it glossy: for shine you need a glossy pouch. Isolated white patches under matte film, however, are a defect, not the matte surface.

One repeat pass — after checking the setting

First compare the thickness on the pouch pack with the laminator's range. On a machine without a temperature control, a pouch thicker than that range is the most common cause of haze. MyPrint's laminators take 80–100 µm (6 in 1 A3), 80–125 µm (SL888 5 in 1 A3 and SL688 5 in 1 A4) or 40–250 µm (LM-330iD). Take any other figures for your machine from its manual.

  1. Check the switch and the setting. The switch must be on hot laminating: in cold mode a thermal pouch comes out as cloudy as it went in and does not stick. If the panel has thickness buttons, choose the one printed on the pack. For a 100 µm pouch on a machine with 80 and 125 buttons: if the first pass was on 80, make the second on 125.
  2. Wait for the ready light. MyPrint laminators take 3–6 minutes to warm up; after changing the setting, wait for the light again. If the first pouches come out clear and haze appears mid-run, the rollers cannot recover their heat: pause, and feed the next pouch when the light is on again.
  3. Feed the same pouch through once more, straight, leading with the edge that was sealed before laminating. If your machine's manual requires a carrier, feed the pouch in it the second time too; if it does not, put nothing around the pouch: a carrier, paper or a second pouch takes heat away. Do not pull the item from the exit.
  4. Lay the item on a flat surface and let it cool. Compare the areas that were milky.

What the control on your machine means

On the panelWhat to select
80 / 125 µmThe button for your pouch thickness: 125 µm is a thickness, not 125 °C.
Temperature in degreesStarting values: 80–100 µm — 100–120 °C, 125–150 µm — 110–130 °C, 175 µm — 120–140 °C, 250 µm — 130–150 °C. Start at the lower end. Haze after cooling — add 5 °C; waves — reduce by 5 °C.
Fixed temperatureThe machine heats for its own pouch range. Run a pouch within that range through again after a full warm-up; replace a thicker one with a thinner pouch.
SpeedThe thicker the pouch, the slower. Then fine-tune the temperature for the paper: one step higher for heavy card.

What the second pass tells you

The haze has gone

So the adhesive was under-heated the first time. Before starting the run, laminate one new sheet at this same setting: it should come out clear first time.

The haze remains

Do not heat it a third time. At the same setting, laminate plain uncoated paper of the same size and weight in a new pouch from the same pack.

↓ No haze on the uncoated paper

The print is the cause. Inkjet prints need to dry for at least a day before hot laminating, dense dark areas longer. If a dry print on photo or coated paper still turns cloudy, use cold laminating film for that paper.

↓ Both samples are cloudy

The pouches or the machine are at fault. Laminate a plain sheet in an 80 µm pouch from a different pack. If it comes out clear, the earlier pouches or their thickness are to blame. If it is also cloudy after a full warm-up, the machine is not reaching temperature: take it to service with both samples.

Waves, large bubbles or changed colour

Do not heat this item again. Waves mean overheating: run the next pouch one setting lower or 5 °C cooler; on a machine without a temperature control, use a thicker pouch within its range. Large bubbles over the print are more often caused by moisture in the print.

Laminate thermal paper, receipts and prints that darken with heat with cold film, which sticks without heat. A print already spoiled by heat has to be reprinted.