25.02.2025

Destructible labels or VOID: what remains after removal?

Destructible labels or VOID: what remains after removal?

If you need fragments after an attempt to remove a label, consider a brittle, destructible material. If you need a revealed VOID message, look for a material with that indication mechanism. Printing the word VOID on ordinary self-adhesive stock or brittle paper is not enough: printing does not create the mechanism.

When choosing self-adhesive paper for labels, filter for the self-adhesive destructible type in the broad photo paper and print media category. The linked page is in Ukrainian. This section also includes ordinary materials; the category name alone does not establish the protective effect you need.

Two different ways to leave an indication

A destructible label breaks within its face material: the material carrying the printed image. In a VOID construction, separation reveals a message or pattern built into the material. Terms such as “seal” or “security label” do not tell you which result to expect.

Before / after schematic, not test photographs

Brittle face material

Before separation

A
–
1
7

Item surface beneath the label

After separation

Removed fragments

–

↑

A
1
7

The same item surface

Indication: pieces of the broken face material. In this schematic, some remain on the item and some have separated.

VOID construction

Before separation

A
–
1
7

Item surface beneath the label

After separation

Removed label

A
–
1
7
VOID

↑

VOID

The same item surface

Indication: a revealed message. This example shows a construction that leaves it on both the removed label and the item surface.

Top view. Removed pieces are shown above without rotation; their positions on the substrate are preserved. Blue represents the label; beige represents the item surface. Fragment boundaries are simplified, not a security-cut layout.

Where will VOID appear?

This depends on the material construction. Some designs do not transfer the indication to the item; others do. Agree on both the message or pattern and where it must be visible after removal.

No transfer to the item

Removed label

VOID

Item surface

No revealed message

Transfer: indication on the item

Removed label

No revealed message

Item surface

VOID

Transfer: indication on both

Removed label

VOID

Item surface

VOID

Schematic examples of indication locations. The particular construction determines removal conditions, the appearance of the indication and the residue; VOID materials do not all leave the same residue.

One 30 × 15 mm layout, two requirements

A hypothetical example: two control labels use the same numbered 30 × 15 mm layout. These dimensions describe the teaching example, not a security label standard. The rectangles above retain its 2:1 proportions.

“We need fragments after removal”

Brittle, destructible paper is a suitable candidate. Confirm that the face material breaks on the intended surface. A sample that peels off in one complete piece has not produced the required result.

“VOID must appear after removal”

You need a construction that reveals this message in the agreed location. Fragments of brittle paper do not meet that requirement, even if VOID was printed on them beforehand.

If the specification separately calls for security cuts, agree on those too: the brittleness of a different material does not establish compliance with that requirement.

For a specific example relevant to the first requirement, consider My Print Eggshell destructible paper (9664). It is brittle paper without a VOID mechanism. A requirement for a revealed message calls for a different material type; a separate VOID range at MyPrint has not been confirmed.

What to check on a printed sample

For the brittle face to break, the adhesive must hold it firmly enough to the item surface. If adhesion is weaker, the label may separate intact. Contamination, texture and an incompatible surface can change the result; the word “destructible” does not replace a trial.

  1. Prepare a finished printed label sample and the same surface it will be used on, with the actual coating, texture and shape.
  2. Prepare the surface, apply the label and allow it to dwell under the conditions specified for that material. There is no universal waiting time or removal force for all labels.
  3. Try separating the sample and compare it with the agreed result: does the face break into fragments or peel off intact? For VOID, also check the message or pattern and where it appears: on the label, the item or both.
  4. If the indication does not meet the requirement, clarify preparation or change the material and surface combination, then repeat the trial. Keep an acceptable sample and record the conditions that produced the required indication.

To indicate opening, the label must bridge the seam

A removal trial checks how the material behaves on the substrate. Opening indication needs another check: the label must connect the two parts that actually separate. A label beside the seam or entirely on the lid does not do this.

Bridges the seam

Lid A ↑

A–17

Base B

Seam A / B

The label adheres to both A and B. Lifting the lid loads the label across the seam.

On one part only

Lid A ↑

A
–
1
7

Base B

Seam A / B

The whole label is on A. The lid can move with it; the label does not connect B to A.

Placement schematic on a closed mock-up. Here the lid moves upwards from the base; test the actual opening motion of your own packaging.

Apply the sample across the intended seam and, after the appropriate dwell, open the mock-up normally. Check whether that motion actually changes the label and produces the agreed indication. An intact sample after this opening has not demonstrated the required indication.

Damage shows that the label's condition has changed. On its own, it does not establish who opened the item, when or why; a control label also does not guarantee that access is impossible.

Agree on the visible result before the print run

Write a short requirement: “On this surface, after this motion, we need fragments” or “We need a revealed VOID message in this location.” Check it on a finished printed sample. That agreement gives you a criterion for selecting the material and accepting the label.